A client of ours has had multiple LV (525V) motor failures since the plant was commissioned (a large smelter).
Our system measurements (over a two week period) show no abnormalities on the system.
Examination of 5 failed motors shows various symptoms (2 rust, 1 interturn, 2 insulation).
Does anyone have experience with problems associated with vacuum switching of LV machines. I have seen problems with travelling wave reflection and voltage doubling off the end of the windings on large MV machines but never on LV machines.