Google doesn't always compensate for spelling errors.
Correct spelling is "Mueller".
That said, 360 brass is 360 brass.
There are alternatives. This page may be on point:
Mike is correct, there is nothing "special" about Mueller 360 brass in terms of composition. Mueller is a high quality supplier of brass products, so their products may be somewhat higher than low cost imports, but you get what you pay for.