How i can receive ASTM materials with out mentioned the year on it according ASME sec 2
Thanks in advance!!
 
Under ASTM rules you are supposed to be working to the most recent published revision.
Under ASME you must list the Code year.

If you are trying to comply with ASME then that must be stated on the MTR.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 