Feb 12, 2013 #1 yonnasz Materials Joined Feb 7, 2013 Messages 1 Location CA Hi Guys, How i can receive ASTM materials with out mentioned the year on it according ASME sec 2 Thanks in advance!!
Hi Guys, How i can receive ASTM materials with out mentioned the year on it according ASME sec 2 Thanks in advance!!
Feb 13, 2013 #2 EdStainless Materials Joined May 20, 2004 Messages 16,351 Location Waukesha WI USA Under ASTM rules you are supposed to be working to the most recent published revision. Under ASME you must list the Code year. If you are trying to comply with ASME then that must be stated on the MTR. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote