metboss
Petroleum
- Sep 12, 2012
- 153
Good day,
We have received API 5CT L-80 Casings and upon review of the MTC (certified true copy by local vendor) it is found that charpy impact test results are not mentioned thereby failing to meeting the requirements of API 5CT code that requires charpy test at 0⁰C.
Based on the above deviation material was rejected. Now, local vendor came with the same MTC with charpy test results being incorporated and I am totally confused.
Please advise what justification should I ask to confirm that certificates are true and not tampered one !!!!
Thanks in-advance
We have received API 5CT L-80 Casings and upon review of the MTC (certified true copy by local vendor) it is found that charpy impact test results are not mentioned thereby failing to meeting the requirements of API 5CT code that requires charpy test at 0⁰C.
Based on the above deviation material was rejected. Now, local vendor came with the same MTC with charpy test results being incorporated and I am totally confused.
Please advise what justification should I ask to confirm that certificates are true and not tampered one !!!!
Thanks in-advance