Plan to use 304 or 316 stainless to fabricate steel structure for a hydraulic lift.
Need reference for non-magnetic steel fabrication (i.e. aluminum alternative).
Plan to use 304 or 316 stainless to fabricate steel structure for a hydraulic lift.