Here is some strange material. apparently this material is
shipped in the solution annealed 1905 deg F (1040C)
hardness 47 HRc (Specification Requires 38 HRc min)
according to the Carpenter Data sheet this material requires
cold or work harden then aged at 800/1200 deg F for 800/1200 deg F for (4) hrs min.
I was supprized that this material was this hard in the
solutioned annealed condition.
is it cold worked at the mill?
Here is some strange material. apparently this material is
shipped in the solution annealed 1905 deg F (1040C)
hardness 47 HRc (Specification Requires 38 HRc min)
according to the Carpenter Data sheet this material requires
cold or work harden then aged at 800/1200 deg F for 800/1200 deg F for (4) hrs min.
I was supprized that this material was this hard in the
solutioned annealed condition.
is it cold worked at the mill?