I have a small motor, core length 50mm, coil projection 20mm both DE and NDE, wound with wire size 2 times 0.14mm wire (2 in parallel), with 469 turns in each half (938 turns in full). I do not have 2 off 0.14mm wire in stock, but I have 2 bobbins of 0.15mm which I would like to use rather buy 0.14mm.
What the new turns should be with 0.15mm wires (2 in parallel)
 
Replies continue below

Recommended for you

If you have 1 bobbin of .2mm that would give you a slight increase from 60.8 to 62 CM. I wouldn't change the turns.
 
it is two sections per coil giving 469 turns , perhaps (2 in parallel) is wrong discription
 