All,
Please see attached photo and let me know if you can identify the root cause of the failure.
Motor data is: 10HP, 460V 3-ph RPM 1755 with Class F insulation
"Throughout space there is energy. Is this energy static or kinetic! If static our hopes are in vain; if kinetic — and this we know it is, for certain — then it is a mere question of time when men will succeed in attaching their machinery to the very wheelwork of nature". – Nikola Tesla
Please see attached photo and let me know if you can identify the root cause of the failure.
Motor data is: 10HP, 460V 3-ph RPM 1755 with Class F insulation
"Throughout space there is energy. Is this energy static or kinetic! If static our hopes are in vain; if kinetic — and this we know it is, for certain — then it is a mere question of time when men will succeed in attaching their machinery to the very wheelwork of nature". – Nikola Tesla