We have two 150 HP 480 VAC motors that had bad bearings that cooked/fused themselves to the motor shaft. Our local motor shop had to cut, heat and pull the internal bearing races off the shaft. This damaged the shaft pulling some of the shaft off in the process of pulling.
My question is: If we have our local machine shop build up the damaged motor shafts by welding and turn (lathe)the built up weld back down will these motors still be reliable? Our local motor repair shop is telling us they will not be reliable after this shaft repair.
These motors are running a critical process that need very reliable motors 24/7 - 365.