Echan
Mechanical
- Apr 11, 2003
- 6
Hello,
Here is the situation. We have a monorail system (35ft span 5 Ton capacity) supported at both ends into the main building structure and by 8 anchor points welded to the main horizontal roof trusses. It has been in operation for 10 years plus and there is no sign of corrosion or cracking or yielding (paint is still like new).
Now here is the problem. A crane inspector had reservations about the 8 bracket anchor points. These are square tubing (2"x2" assuming 1/4" thickness and 7" long) welded between two 1/2" plates where the bottom is mounted to the main horizontal I-beam (w12x26) with 4 - 3/4" grade 5.2 bolts (Sp=85 Kpsi) and the top is welded to the roof trusses. We had multiple inspectors on site inspect our cranes and this is the first time that this was brought up. The square tubing seams to have been installed at an angle from that start with the bottom being flat with the I-Beam and the top being mounted at a small angle to the roof trusses.
Brackets looks like this:
____
\
|
|
---
There is approximitly 1/2" difference between the top and bottom and seems have been pre-bent or bent during installation.
I have gone through stress calculations for the welds, bolts, beam and tensional stresses in the square tubing.
All ok.
My question is what is the best way to calculate the square tubings stress with the bend in it.
Thanks
Echan
Here is the situation. We have a monorail system (35ft span 5 Ton capacity) supported at both ends into the main building structure and by 8 anchor points welded to the main horizontal roof trusses. It has been in operation for 10 years plus and there is no sign of corrosion or cracking or yielding (paint is still like new).
Now here is the problem. A crane inspector had reservations about the 8 bracket anchor points. These are square tubing (2"x2" assuming 1/4" thickness and 7" long) welded between two 1/2" plates where the bottom is mounted to the main horizontal I-beam (w12x26) with 4 - 3/4" grade 5.2 bolts (Sp=85 Kpsi) and the top is welded to the roof trusses. We had multiple inspectors on site inspect our cranes and this is the first time that this was brought up. The square tubing seams to have been installed at an angle from that start with the bottom being flat with the I-Beam and the top being mounted at a small angle to the roof trusses.
Brackets looks like this:
____
\
|
|
---
There is approximitly 1/2" difference between the top and bottom and seems have been pre-bent or bent during installation.
I have gone through stress calculations for the welds, bolts, beam and tensional stresses in the square tubing.
All ok.
My question is what is the best way to calculate the square tubings stress with the bend in it.
Thanks
Echan