You have the right paragraph for flanged valves. It is 6.2.2. It says, "Flanged ends shall be prepared with flange facing, nut-bearing surfaces, outside diameter, thickness, and drilling in accordance with ASME B16.5..."
Flange facing is applicable
nut-bearing surface is not applicable
outside diameter is not applicable
thickness is not applicable
drilling is applicable, but also meets the additional notes in paragraph 6.7.