Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Monitoring Concrete Cure/ thermocouple

Status
Not open for further replies.

ToadJones

Structural
Jan 14, 2010
2,299
Does anyone out there have any information on monitoring the temperatures on a mass concrete pour using a thermocouple?
 
Replies continue below

Recommended for you

from my General Notes...


MASS CONCRETE

CONCRETE POURS HAVING A TOTAL VOLUME IN EXCESS OF 5 CU-M AND A MINIMUM DIMENSION IN EXCESS OF 3 FT SHALL BE CONSIDERED AS MASS CONCRETE

CONCRETE WORK SHALL COMPLY WITH THE RECOMMENDATIONS OF ACI COMMITTEE 207

CEMENT TYPE FOR MASS CONCRETE SHALL BE TYPE LH UNLESS APPROVED BY THE [CONSULTANT | ENGINEER]

MAXIMUM AGGREGATE SIZE SHALL BE 2" UNLESS APPROVED BY THE [CONSULTANT | ENGINEER]

PROVIDE PAIRS OF THERMOCOUPLES IN THE CENTRE OF MASS OF THE CONCRETE POUR

PROVIDE SURFACE THERMOCOUPLE PAIRS AT THE TOP SURFACE OF THE CONCRETE POUR DIRECTLY ABOVE THE THERMOCOUPLE PAIR AT THE CENTRE OF MASS, NEAR THE CENTRE OF TWO ADJACENT VERTICAL FACES AND AT ONE CORNER (5 SURFACE PAIRS TOTAL)

SURFACE THERMOCOUPLE PAIRS SHALL BE PLACED 2" FROM THE OUTSIDE SURFACE AND AT MID DEPTH OF THE CONCRETE POUR

THERMOCOUPLE PAIRS SHALL BE SEPARATED BY A DISTANCE OF APPROX 4'

MAXIMUM TEMPERATURE AT THE CENTRE OF MASS SHALL NOT EXCEED 50%%DC

MAXIMUM TEMPERATURE DIFFERENTIAL BETWEEN THE CENTRE OF MASS AND THE CONCRETE SURFACE SHALL NOT EXCEED 25%%DC

CONTRACTOR SHALL PROVIDE A PROCEDURE OUTLINING PROPOSED METHOD FOR MAINTAINING TEMPERATURE REQUIREMENTS FOR REVIEW BY THE [CONSULTANT | ENGINEER]

 
Dik-
good stuff.
What is "%DC"?

Does any old thermocouple wire work?
 
They have thermocouple wire already 'pre-fabbed'... the %%DC is for Autocad %%D yielding a 'degree' symbol and the C for Celcius...

You need to talk to someone about logging the information... most test agencies have this type of equipment. Unfortunately, for the project I did the notes up for, they testing agency hadn't a clue about what they were measuring.

Dik
 
Yes.
I realize that now....I use ALT+0186 to make a º symbol.

We are purchasing the logging device ourselves and monitoring our own pours.

 
Good... I know where I can borrow one <G>...

Since I've been with my present employer (2 years), they have purchased a laser distance measureing device (Hilti), a temperature measuring device (Laser pointer type) and temperature and humidity data logging devices... I had these prior to starting with them and they have found them so useful. I still have a laser level (also Hilti) and a 5 sec theodolite (70 years old and mint).

We don't have thermocouples or logging device (likely 8 channel) but we have enough electrical and electronic dudes that we could glue one together...

Dik
 
Dik-
As long as I can figure out how to do this, we figure it is better to spend some money to the equipment rather than pay a testing company...at least this way we have the equipment to show for it. The stuff really isn't too expensive relative to the projects.
It sounds like you just literally hook the thermocouple wires to the data logger and let 'er rip.
 
That's about it... Good luck.

Dik
 
Dik-
Can I blame you if it doesnt work?
 
No... but you can use me as an excuse...

Check your thermocouples before you cast the concrete... for continuity as well as function and correlation. If this is OK, then there's no reason it shouldn't work. If I get a chance, I'll talk to one of the electrical dudes here to see about the data logging stuff...

Dik
 
Calibrate your readout units as well. We have some 10 of these on site and they all read different - about 1 to 2 degrees. We have calibrated vs 40degC temp. Be careful about protecting them - depending on the installation, vibration during placement have been known to cut the wiring. Shouldn't happen but sometimes "... .... .. -" happens.
 
BigH-
Is 1 or 2 degrees that big of a deal?
Will the unit come with instructions for calibrating?
We are purchasing the logger from Omega.
 
Calibration is good... but the biggest concern is the temperature differential between the centre and the outside. My experience has been with cold weather, and it is possible that hot weather can provide a concern also. Only in the event of a problem is the calibration an issue... I wouldn't normally lose sleep over a couple of degrees, but, I do appreciate precision and care.

Dik
 
Logger is running and providing output just the way some literature I have read on the subject says it should.
 
ToadJones - normally I would say not - but we have, due to "thermal analyses" very stringent maximum temperatures of the concrete we are placing. Designers worried about thermal cracking - due to a "new" analysis, the max temps dropped 2 degrees C.
 
Big H-
We did calibrate the unit.
The thing that was throwing me off was apparently the logger itself creates some heat and reads a few degrees F higher than a probe left in the air nearby the unit. The mfg. assured me that this was normal.

THanks
 
Generally looking at relative temperatures... if both are off a couple of degrees, they're almost the same...
 
Status