Jul 25, 2018 #1 Vikumar Mechanical Joined Mar 29, 2018 Messages 7 Location US Can anyone explain me what is the difference between Monel 400 & K400? Are both represents the same with different name?
Can anyone explain me what is the difference between Monel 400 & K400? Are both represents the same with different name?
Jul 25, 2018 1 #2 btrueblood Mechanical Joined May 26, 2004 Messages 10,034 Location US Not heard of K400 before now, but K500 is a precipitation-hardenable version of 400, i.e. added Ti and Al to form precipitates, though at the cost of slightly lower corrosion resistance. https://en.wikipedia.org/wiki/Monel Upvote 0 Downvote
Not heard of K400 before now, but K500 is a precipitation-hardenable version of 400, i.e. added Ti and Al to form precipitates, though at the cost of slightly lower corrosion resistance. https://en.wikipedia.org/wiki/Monel
Jul 25, 2018 1 #3 bimr Civil/Environmental Joined Feb 25, 2003 Messages 9,381 Location US Another useful characteristic of the Monel Alloy K-500 is that it is virtually nonmagnetic. Monel Alloy 400 does not have nonmagnetic characteristics. specialmetals.com Monel Alloy 400 Monel Alloy K-500 Upvote 0 Downvote
Another useful characteristic of the Monel Alloy K-500 is that it is virtually nonmagnetic. Monel Alloy 400 does not have nonmagnetic characteristics. specialmetals.com Monel Alloy 400 Monel Alloy K-500
Jul 26, 2018 Thread starter #4 Vikumar Mechanical Joined Mar 29, 2018 Messages 7 Location US Thanks Btrueblood and Bimr for your reply on my query. Upvote 0 Downvote