tab1999;
Hot cracking is a very real possibility when welding with Monel welding filler metal. Even when welding with appropriate Nickel base filler metals or Nickel filler metals. hot cracking in the Monel HAZ can be a problem due to the large liquidus to solidus temperature range of Monel (even when properly cleaned).
Cracking in the HAZ of Monel castings is a greater possibility. Depending on the melting practice used for the Monel casting it may prove unweldable.