I am looking for resources that would have listings of physical properties of molten sulfur -web sites, books, articles, etc. I specifically need thermal conductivity info. Thanks in advance for the help!
 
Replies continue below

Recommended for you

"The Sulphur Data Book" compiled by Freeport Sulphur company, edited by William N. Tuller and published by McGraw Hill in 1954 may be dated but is still an excellent source of info.
Thermal conductivity of liq sulphur varies from 0.077 BTU/hr2 F @ 260F to 0.088 @ 380F. Not quite linear relationship.
K
 