Feb 6, 2018 #1 gearteeth Materials Joined Jul 24, 2014 Messages 17 Location US Can any one offer up useful resources on molten salt corrosion within delayed coking units? Process side, not fire side. I have some failure analyses, internal company documents, and G.Y. Lai's book on high temperature corrosion.
Can any one offer up useful resources on molten salt corrosion within delayed coking units? Process side, not fire side. I have some failure analyses, internal company documents, and G.Y. Lai's book on high temperature corrosion.