If anybody know the modulus of Elasticity for Bolt M14x1.5 10.9 and steel tube E235 +C (EN 10305-1:2002) or St35BK (DIN 2391-2)

Thanks
 
Replies continue below

Recommended for you

Room temp values
plain carbon, low carbon steel 27.9ksi
plain carbon, high carbon steel 29.9ksi
(the breakover is about 0.30-0.35% C)

alloy steels, high carbon (4140, 4335) 31.6ksi

These are from the ASM book on high temperature properties of ferrous alloys.

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
 