Modelling a Composite

Status
Not open for further replies.

glassyoffshore

Computer
Joined
Jan 5, 2004
Messages
20
Location
IE
Hi,
I'm want to model a unit cell of a compostie material in 2d. Is this a contact problem? Any tips would be great.
Thanks,
 
Hey,

If ur composite is a perfectly bonded, then u can use the *TIE command.
If it is not, then it is a contact problem.

have fun,
Nishanth
 