Hi!

Im new to this forum and this is my first question.

How does the fibres influence the result of an modal analysis of fibre reinforced polymer? The parts that i'm simulating has a complex geometry with lots of small ribs. Moldflow analysis show that the directions of the fibres vary from coherent to incoherent. I guess that the stiffness vary with the directions and the coherence of the fibres but i don't know the influence of the result.

Are there any litterature on this topic?

Regards/
OlofG
 
Probably need to start simply with a text on orthotropic plates, but your basic assumption is correct. Stiffness varies with direction of the fibers. You can probably find some graphs online at various University websites. Try University of Delaware or University of Illinois Urbana-Champaign. Both have large departments working in this field.

I will say, however, that it sounds like you are using short fibers as opposed to continuous fibers. Short fibers will generally behave more like an isotropic plate since the direction of the fibers is difficult (impossible) to perfectly predict. In this case, you generally "smear" the properties of the fiber and resin and use these "smeared" propeties in an isotropic plate formulation.

Garland E. Borowski, PE
Borowski Engineering & Analytical Services, Inc.
Lower Alabama SolidWorks Users Group
 
Status