I received some very good info re. MOC from this thread: thread124-190648. However, further investigation has revealed how difficult they are to get hold of!
Can anyone advise on the suitability of glass lined reactors for the following process conditions:
70% Nitric acid @ 121ºC (BP).
The following issues are associated with using stainless / duplex / noble metals:
304L - unsuitable
Titanium - suitability questionable. Corrosion rates are quoted from 0.05 - 0.9 mm/year under these conditions!
Hastelloy G30 - Very scarce
Proprietary duplex grades - Only used for certain applications e.g tubing or require very large orders
Zirconium - Cost?
Considering the above, glass lining seems to be the best option.
In addition, the vessels will be trace-heated with possible cable sheath temperatures of 450ºC. Can this accelerate corrosion? And is this an issue if you have glass-lining?
Thanks in advance
Can anyone advise on the suitability of glass lined reactors for the following process conditions:
70% Nitric acid @ 121ºC (BP).
The following issues are associated with using stainless / duplex / noble metals:
304L - unsuitable
Titanium - suitability questionable. Corrosion rates are quoted from 0.05 - 0.9 mm/year under these conditions!
Hastelloy G30 - Very scarce
Proprietary duplex grades - Only used for certain applications e.g tubing or require very large orders
Zirconium - Cost?
Considering the above, glass lining seems to be the best option.
In addition, the vessels will be trace-heated with possible cable sheath temperatures of 450ºC. Can this accelerate corrosion? And is this an issue if you have glass-lining?
Thanks in advance