Hello,

Here is one more problematic I would like to get more info or some opinions.

I have heard that with mixing up the electrolyte during charging the charge time can be reduced with up to 30% and this mixing is carried out in big battery station by air.

I read somewhere that the mixing up of the electrolyte could be provoked electrycally by applying short negative voltage pulses during charging.

What is your opinion - it might be true or it is rather a myth and it case it would work if it will reduce the life cycle of the battery by applying these pulses ( effectively changing polarity ) for a short time?

I have not found other source to verify this method and my own electrochemistry knowledge is limited to make directly the consequence.
 
Replies continue below

Recommended for you

I'm not sure that I would recommend air mixing, since that might result in entrained air bubbles, which could cause plate problems. Maybe a slow rocking motion might be plausible.

However, I would caution against trying to "speed up" the charging process, as that might cause uneven restoration of the plates, resulting in an overall lower reliability.