tolchijb
Structural
- Jun 19, 2004
- 69
Is it standard practice in high seismic regions to specify A706 rebar only or do you only specify A706 at ductile elements and use A615 everywhere else. If you do mix rebar, how is it delineated as different in the field other than standard bar markings that are not going to scream that this rebar is different?