Hi,
We have cross Country Petroleum pipelines that share ROW with HT lines. All our pipelines are cathodically protected (Coating is 3LPE). We have observed Pipeline AC pick up of 17 VAC at one test station where the soil resistivity is 500 Ohm-cm. Temporarily, we have installed 4 nos (20kg) Zn anode(Directly to Pipeline) for grounding.After Zn anodes Installation, the AC pickup at that Test Station drops to 6 VAC. Now we are planning for installation of Polarization cell at that Test Station.
My Question is,
1. Whether the AC current induced in our Pipeline will ground through the Zn anode or travel through the pipeline?
2. How to bring down the AC pickup below 2VAC?
We have cross Country Petroleum pipelines that share ROW with HT lines. All our pipelines are cathodically protected (Coating is 3LPE). We have observed Pipeline AC pick up of 17 VAC at one test station where the soil resistivity is 500 Ohm-cm. Temporarily, we have installed 4 nos (20kg) Zn anode(Directly to Pipeline) for grounding.After Zn anodes Installation, the AC pickup at that Test Station drops to 6 VAC. Now we are planning for installation of Polarization cell at that Test Station.
My Question is,
1. Whether the AC current induced in our Pipeline will ground through the Zn anode or travel through the pipeline?
2. How to bring down the AC pickup below 2VAC?