Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Mistake proofing 1

Status
Not open for further replies.

QAgirl

Automotive
Joined
Jan 9, 2003
Messages
4
Location
US

We are a commercial heat treating plant who is currently undergoing our QS9000 registration. I am having trouble defining mistake proofing. None of he manuals that we have give a specific definition, only that verification by an operator ( visual ) is not enough. Any information on mistake proofing would be appreciated.
Thanks
 
Generally speaking, mistake-proofing (also called poka-yoke, and spelled in a variety of ways) involves designing the parts, assemblies, and fixtures such that a defective part cannot be used or made. Some examples include:

- Using locating holes and pins to orient a part in the correct position.
- Designing a fixture so that an incorrect size part won't fit.
- Designing tooling so that it cannot physically make a defective part.

The main focus should be (1) don't make a bad part, and (2) parts and assemblies should be "self-inspecting".