I have a job where a couple of drill-in & epoxy anchor rods where moved due to hitting rebar in the drill hole. There is now about 1" seperation between the original hole (approx 1/2 the specified depth) & the new hole. What is the best material for filling the unused hole?
 
You can use the same epoxy that was used for the anchors. It can be supplemented with oven dried sand which will reduce shrinkage.
 