Hi

Do dimension (tmin) consider thicknesses of parts corroded in UW-16 or nominal thicknesses?

Thanks
Torsani
 
Replies continue below

Recommended for you

tmin is defined in terms of t,tn and te, and all of them are nominal thicknesses as called for by code in UW-16.

prex

Online tools for structural design
 
See SecVIII Div1 Appendix 3,Thickness of Vessel Wall.
 