In case of ASME U-Stamp Vessel, I found the calculated thickness of an ellipsoidal head per ASME Sec. VIII Div. 1, Appendix 1-4(c) less than minimum thickness after forming. However, norminal plate thickness is more than the calculated thickness. Is this acceptable for ASME U-Stamp Vessel? Please advise.
 
Replies continue below

Recommended for you

May you clarify your doubts?
If I understand you correctly, you have the actual minimum thickness of head (assuming corrosion allowance doesn't matter) higher than the minimum calculated thickness, so you are OK. And of course plate before forming must be thicker, as thickness reduces at some locations in the forming process (and increases at other locations).

prex

Online tools for structural design
 
Adding to prex's post what you have gotten into is the forming allowance for the particular type head you have.
A good point is to tell the head manufacturer the minimum thickness needed as per design and let him pick the starting plate thickness. You will nearly always get a little extra thickness and unless you are designing a spaceship you will need it later on.

Checkout the following site as it gives a little in site in to the process and has downloadable spreadsheets for heads.

 
Have you reviewed UG-79 and the referenced paragraphs?

See Appendix 3 Thickness of Vessel wall.
 
Sorry for my mistake. The correct post should be "minimum thickness after forming less than calculated thickness (include corrosion allowance)".

The manufacturer informed me that the minimum thickness of head is before forming. Is this acceptable?

Please advise me.
 
No, it isn't.
You could start thinking to what type of analysis or test could be used to demonstrate the acceptability of the head, but of course this would cost much more than doing another one (hope it is not already welded to shell, but even in that case...)

prex

Online tools for structural design
 
Thank you prex. Finally, I find out that the calculated thickness (exclude corrosion allowance) is less than thickness after forming. In this case, it is acceptable.
 