Yesterday at 8:03 PM #1 Cormet Petroleum Joined Jul 3, 2007 Messages 11 Location US This just came in..... low Cr piping welding (1¼Cr, 2¼Cr, 5Cr and 9Cr), We need two minimum PWHT cycles Is this a code requirement from B31.3??? Thanks,