Working on an ASME vessel alteratation, adding a 10" sch 160 nozzle in the top of a 2:1 ellipitical head.
What would be considered a reasonable minimum distance between the weld on the shell to the next weld on the nozzle?
We are in a very tight space. Some on the project feel that having a nominal 2 to 3" long nozzle projection from the head is acceptable.
The head material is SA516-60 normalized and welding will be 100% radiographed, nozzle SA-106-B
What would be considered a reasonable minimum distance between the weld on the shell to the next weld on the nozzle?
We are in a very tight space. Some on the project feel that having a nominal 2 to 3" long nozzle projection from the head is acceptable.
The head material is SA516-60 normalized and welding will be 100% radiographed, nozzle SA-106-B