Zaheer_Ahmad_Raza
Mechanical
We have observed severe pitting (Remaining Thickness approaching Minimum Required Thickness of Top Shell Course) only in top 6" of top shell course of a Tank. Remaining Portion of the Shell Course is health. Now we have to repair that portion of the shell course.
Can we Replace the entire top 12" of the Top shell course as per API 653 Clause 9.2.2 satisfying all the requirements of weld spacing or do we need to replace the entire shell course?
Furthermore, does API 653 limit the extent of build up to be carried out if we decide to build up entire top 6" of corroded shell course?
Can we Replace the entire top 12" of the Top shell course as per API 653 Clause 9.2.2 satisfying all the requirements of weld spacing or do we need to replace the entire shell course?
Furthermore, does API 653 limit the extent of build up to be carried out if we decide to build up entire top 6" of corroded shell course?