I am looking for the minimum bend radius of Stainless 305. Sheet thickness is .008". I want to do ~200 degree bend.

Does anyone have a formula? I was looking in the Machinery Handbook but couldn't find it.

Thanks in advance.

Josh
 
weirdo: I think this is what your looking for
Sheet metal bend allowance: