We have an 8 inch slab with rolling equipment and enhanced aggregate interlock utilizing reinforcing crossing the control joints.

i received a mix design that utilizes #78 pea gravel. my gut tells me to reject this for the aggregate interlock issue the pea gravel will likely create, given that its so small.

Is there a minimum aggregate size that should be specified for slabs using aggregate interlock?
 
You should use the maximum sized aggregate to reduce shrinkage. For most small slabs I use 3/4" and for 8", depending on the use, I would consider 1-1/2" aggregate. Pea gravel should not be used. Reject...
 
i received a mix design that utilizes #78 pea gravel. my gut tells me to reject this for the aggregate interlock issue the pea gravel will likely create,

I agree with you.
Two reasons;
- Aggregate interlock ( so load transfer) less effective,
- The size of aggregate ( in this case ,#78 pea gravel ) more prone to shrinkage.
Use greater max. size aggregate ( say 1.5 in )

Agree with Mr DIK and a pink star for prompt respond.
 
Too small. 20mm minimum, or preferably bigger as suggested. above.
 
As a contractor I'll sometimes use pea gravel (10mm) in areas of high congestion or those that are difficult to vibrate and where self-consolidating concrete is not an option. But none of that is applicable to a slab-on-grade. I would expect a 3/4" max aggregate size for most slabs-on-grade unless they were rather large and a larger aggregate size was justified. Pea gravel seems like a problem waiting to happen especially if coupled with less than ideal curing conditions, which if we're being honest with each other, is almost always (i.e. a proper wet cure is doubtful).

@Tomfh just because it's confusing in this context we should be clear, I imagine you to mean 20mm (3/4") minimum, maximum aggregate size :ROFLMAO:
 
Yes a minimum maximum of 20mm, what’s not to understand?? 🤣
 
As a contractor I'll sometimes use pea gravel (10mm) in areas of high congestion or those that are difficult to vibrate and where self-consolidating concrete is not an option.
A slab on grade is not likely to have high congestion of rebar... The use of reinforcing in slabs on grades is open to discussion.

Due to the 'rounded' nature and size of pea gravel, it's just a bad idea under any circumstance.
 