I urgently need to find 1/4" diameter cylindrical fuses with IR rating at least 3kA on 208 VAC (better 5kA or higher).
I've found one in Ferraz Euro Fuses, however I need one which is UL or CSA aproved (I am in Canada).
Does anybody have suggestions?
Thanks in advance.
 
Replies continue below

Recommended for you

the GGC fast acting series through 10A are 10kA I.R. @ 125VAC and are CSA/UL

the GAB fast acting series through 15A are 10kA I.R. @ 125VAC and are CSA/UL

David Baird
mrbaird@hotmail.com

Sr Controls Engineer

EET degree.

Journeyman Electrician.
 
Thank You, Busbar.
The last one may be acceptable, if nothing better is found.
Still, keep my question in mind, please.
 