AWS D1.1, Annex I has an approach that is more conservative than other welding standards I've worked with. It is based on the chemistry (carbon equivalency) of the base metal, the potential for introducing hydrogen into the weld pool, and the degree of restraint. Considering the thickness you are welding, I would consider it to be highly restrained.
Best regards - Al