Mohamed_AN
Mechanical
- May 29, 2025
- 1
After initial adjustment, the minimum gap setting on our Danieli pinch rolls drifts during operation, causing misalignment and poor wire guidance. Inspections (bolts, bearings, alignment) show no obvious faults. Seeking expert insights on root causes and corrective actions.
Detailed Description:
- Equipment:
- Danieli pinch rolls in a wire rod mill.
- Function: Guides the wire between passes with adjustable min/max roll gaps.
- Problem:
- After few hours (2 or 3h) of operation, the minimum gap widens unexpectedly (Problem occurs when rolling small diameters 5.5 and 6mm).
- Leads to vibrations, wire twisting, or uneven wear.
- Issue persists despite re-tightening bolts and checking pneumatic actuator.
- Suspected Causes (Need Validation):
- Thermal expansion of components ?
- Wear in internal adjustment mechanisms (e.g., screws, shims)?
- pneumatic system fluctuation ?
- Already Checked:
- Bolt torque, bearing/bushing, actuator condition, roll alignment.
- No visible damage or lubrication issues.
Questions for Experts:
- Has anyone faced similar gap drift with Danieli rolls? How was it resolved?
- What components should we inspect more closely (e.g., adjustment screws, sliding blocks)?
- Are there preventive maintenance steps to mitigate this (e.g., recalibration frequency)?
- What components should we inspect more closely (e.g., adjustment screws, sliding blocks)?
- Are there preventive maintenance steps to mitigate this (e.g., recalibration frequency)?