Is it ok to use 100% argon gas to weld mild steel plates ?
Plate thickness is 1/4" to 3/4".
Currently we have no mixed shielding gas such as 80/20.
We are using solid wire .
We noticed during fit up that some of the tack welds did
not hold.
Is there a proceedure to follow that will allow us to
maintain structural integrity, while using this
combination of parent metal/ gas / & wire ?
Plate thickness is 1/4" to 3/4".
Currently we have no mixed shielding gas such as 80/20.
We are using solid wire .
We noticed during fit up that some of the tack welds did
not hold.
Is there a proceedure to follow that will allow us to
maintain structural integrity, while using this
combination of parent metal/ gas / & wire ?