Is it a relation between MFI of plastic and shrinkage of plastic? (At least gualitatively)
Thanks
 
Replies continue below

Recommended for you

I have found that if a material has a low melt flow rate, hence is very viscous when molten, then it is harder to 'pack out' during the packing stage of the molding cycle and therefore harder to prevent sinking.

 