Dear All,

i am looking for means or ways to remove the HVOF coating. Any suggestion would be of great help.

 
Replies continue below

Recommended for you

on 13-4 Cr Ni SS plate.
 
IF the coating is of poor quality then shot blasting may remove it.
If it is a good coating with good surface prep then grinding is about the only way to get it off.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
What Ed said. The Cr in your powder mix makes a chemical etch difficult (likely to etch the substrate).
 
is it advisable to heat up to 400 Degree and soak for 2-3 hours and remove my chipping?
 