I would like some advice on methods to use to calculate steam pressurization accident scenario. The end result is to size a pressure relief device for safety. I am pressure casting metal using water cooled induction coils
System:
Vacuum Chamber - 8.3ft^3
Heat Source - Crucible at 1000 C, diam=4inches
Induction Heating Coils ~ 0.75 inch away from crucible, water cooled at 2-5 gpm, 0.5in diameter copper tubing
I believe that the likely accident scenario is a pinhole in the copper line spraying on the hot crucible.
I have done some research and have found information on Liedenfrost Temperature methods may be applicable.
System:
Vacuum Chamber - 8.3ft^3
Heat Source - Crucible at 1000 C, diam=4inches
Induction Heating Coils ~ 0.75 inch away from crucible, water cooled at 2-5 gpm, 0.5in diameter copper tubing
I believe that the likely accident scenario is a pinhole in the copper line spraying on the hot crucible.
I have done some research and have found information on Liedenfrost Temperature methods may be applicable.