jimbofitz
Electrical
- Aug 6, 2007
- 47
The Metglas cores we are using in our transformer assemblies are flaking (delaminating and breaking off) due to handling while we build the transformer. I would like to coat the surface of them to prevent this from happening. I have a sample of Dolph AC-46 air dry varnish on the way to try out. Has anyone has similar problems with these cores and solved this problem? I can't use our typical varnish system because these cores are sensitive to temperatures above 150 deg C. Another issue is the buildup of this coating is going to be limited as the mechanical design is pretty tight already.
All comments and suggestions are appreciated.
Thanks,
Jim
All comments and suggestions are appreciated.
Thanks,
Jim