Oct 26, 2006 #1 Flesh Materials Joined Jul 17, 2003 Messages 108 Location US I can't find a good explanation for what this stuff, meonite, is. Can anyone go into further detail other than "it is a gray iron". History? Chemistry? Whose trademark/patent?
I can't find a good explanation for what this stuff, meonite, is. Can anyone go into further detail other than "it is a gray iron". History? Chemistry? Whose trademark/patent?
Oct 26, 2006 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Do you mean Meehanite? http://www.meehanite.com/ Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
Do you mean Meehanite? http://www.meehanite.com/ Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Oct 26, 2006 #3 arunmrao Materials Joined Oct 1, 2000 Messages 4,758 Location IN It is a patented gray iron having Type A graphite in a pearlitic matrix. Upvote 0 Downvote
Oct 27, 2006 Thread starter #4 Flesh Materials Joined Jul 17, 2003 Messages 108 Location US I was not sure of the spelling, but "Meehanite" appears to fit my description. Thank you both. Upvote 0 Downvote