Does anyone knows what is the minimum and maximum melt temperature for EP332L Polyproplene.

I need the melt temperature in order to figure/determine the holding pressure graph i.e process window.

Thanks

Clifton
 
Dear Pat,

Thanks for your reply... I have the following article but unfortunatley i had no luck....


Mainly the melt temperature should be around 230 deg celcius.

But in order to do the holding pressure graph i.e process window i need the minimum/maximum.

Thanks
 
From the link above - Table on page 15

Flow Characteristics Melt Temperature
Range, °F (°C)
Low flows 475-500 (246-260)
Medium flows 445-475 (228-246)
High flows 400-445 (200-228)
Extra high flows 385-420 (200-215)
Ultra high flows 370-385 (185-190)

H

 
Yes I read it...

but it does not specific for Polyproplene EP332L.

Thanks
 
That is exactly why you need to get the information from the manufacturer. The data you request varies from grade to grade.

We can give general replies, but t answer accurately, we would need to determine who the manufacturer is then contact them or we would need to go to matweb for you. You can just as easily do it for yourself.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
mmm ic thanks for your kindly Help...

The manufacturer is Mopelan Basell....

Regards
 
If you log in to their website (I believe creating an account is free) you can access their data sheets for the material.
 