enginesrus
Mechanical
I've wondered why there are some manufactures using cast iron for the topic of this thread. Not so for larger engines but for medium speed ones. Since cast iron is so difficult to repair I personally don't see the logic other than maybe manufacturing cost, I know if I was in a position to purchase such engines I would take fabricated over cast iron every time. Can anyone spread more light on this?