Hi All,
I am qualifying a welding procedure for both 10" and 24" pipe using ASME 31.3. This is the code the company recommend.
Please can any one assist me on the position to cut the weldment for the Tensile, Impact, Hardness, macro, side bend and all weld metal test from according to B31.3.
I will also appreciate if anyone can assist me with an ASME B31.3 welding procedure qualification mechanical test request form
I am conversant with ISO standard but not with ASME B31.3
Thanks
Chitessy
I am qualifying a welding procedure for both 10" and 24" pipe using ASME 31.3. This is the code the company recommend.
Please can any one assist me on the position to cut the weldment for the Tensile, Impact, Hardness, macro, side bend and all weld metal test from according to B31.3.
I will also appreciate if anyone can assist me with an ASME B31.3 welding procedure qualification mechanical test request form
I am conversant with ISO standard but not with ASME B31.3
Thanks
Chitessy