Does any one know where I can find the shear strength and bearing stregth of 44W steel. Any help would be greatly appreciated.


Alex C, EIT
 
Replies continue below

Recommended for you

Mechanical Properties 44W/300W:
Tensile: 65 to 85 ksi
Yield: 44 ksi min
Elongation: 20% min in 8” 23% min in 2”


Wes C.
 
Usually, shear strength and bearing strength would be taken as the strength of an object, not of the steel itself. Anyway, check the different building codes- LRFD, for example- for shear and bearing strength of beams, etc.
 