Does any one have a link to data the mechancial properties of Stainless steel as a function of temperature.
I'm trying to determine what will happen to the strenght of stainless springs when used for fixturing in a brazing furnace that can get up to 1000 degrees C.
 
Replies continue below

Recommended for you

ASM speciality handbook"Heat Resistant Material" chapter Elevated temperature mechanical properties of stainless steels pp123-145.