Dear All

please help me to provide the specific reason of not getting the desired mechanical properties after HQT of AISI 4130 pipe of 3 inch

parameters taken for HQT
Process Temperature ⁰C Soaking Time (Hrs)
Normalizing 900 2:00
Hardening 860 2:00
Tempering 550 2:30

Results achieved are attached

 
 https://files.engineering.com/getfile.aspx?folder=572970f6-5289-4cd2-b2c9-0db9863e6b18&file=Mechanical_results.bmp
Replies continue below

Recommended for you

Dear Saurav,

Check the furnace parameters and also carry out PMI of the material. Your answer might lie there.

Regards.

DHURJATI SEN
 
What is the pipe wall thickness?

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
In looking at the attached results, I would first follow Dhurjati's suggestion, we got so much different results from trial 1 and 2 (if you used a same temper temperature)!
 