Is it possible to obtain mechanical properties (yield point, resistance, elongation, etc), or some of them, even approximately, by knowing the chemical composition of a steel plate?

In this case it is a very low carbon steel, used to build a galvanizing pot, and its compositions is(%):

0.04C + 0.28Mn + 0.019P + 0.008S + 0.063Al

I don't need a very accurate value. The steel supplier is unknown.


Thanks in advance,

Heyner
 
The chemical composition can be used to determine the type of steel, and depending on the heat treatment condition one can attempt to establish a range of mechanical properties.

Your reported chemical composition indicates a low carbon steel. The Al addition implies a killed steel (deoxidized). At my present location, the only information I can find regarding this low carbon steel is as follows;

Assuming a 1006 CS, hot rolled;

UTS ~ 60 ksi
Yield Point - ~40 ksi
Elongation (2" gage) ~ 30%

These are ball park estimates.
 
Hey, thanks again, it is a great tip!

Heyner
 
We usually use the following formula to estimate the Minimum tensile strength of a steel
Min. tensile strength, kgf/mm2 = 20 + 100(%C)
in your case, it's approx. 34 ksi. This should be the figure to be considered in your design.

Besides, from safety pont of view, usage of an unknown steel, should comply the following;
- it does not subject to temp. more than 350 C
- do not weld it

Best regards,
ct
 
Very important tip, thanks!

Heyner
 
While chemistry and composition of raw ingredients affects the mechanical properties of finished products, the fabrication process also affects these properties, whether its metals, polymers, or inorganic non-metallic materials (ceramics).
 