dreamschool
Mechanical
I noticed a decreasing in the mechanical properties after forming the pipe for the Spiral Pipes only …about 25%.... Why do we have this decreasing?
Any body Know about “Bauselirger Effect” Phenomena?
Regards,
Any body Know about “Bauselirger Effect” Phenomena?
Regards,